Originally Posted by therivermonster View Post
Hey, Red! Thank you so much for this post. As I mentioned in my reply to Jesus, I am ready to try another body filler. I think that I'll give Rage Gold a try. Do you feel that the Rage product has a longer open time compared to regular Bondo?
The open time depends more on the temp and how much catalyst you rage gold is about the same as the other brands. where you will notice the difference is that it has a finer texture so it spreads smoother and it sands eaiser. ALso your sand paper will last longer.

Most of the time you will get a better surface with a putty knife than with a bondo spreader. also if you take a plastic bondo spreader and "sharpen" it on some sand paper, which will require you to take it up to 600 wet dry, you will also get a better surface.