sailah OP
Lampin' it
 
sailah's Avatar
 
Joined: Aug 2005
Location: Turning expensive metal into scrap
Oddometer: 5,499
Thanks joe. it has a lot of porosity I think due to me using most of the argon flow to the back of the weld. My practice welds looked much more professional.as long as it holds it will be fine.

I'm going to make the heat shield and seat pan from carbon fiber unless I can get some thin aluminum. I have some days off this week so I'll crank out the work.
sailah is online now   Reply With Quote
 

Share

Thread Tools Search this Thread
Search this Thread:

.
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On

Forum Jump


Times are GMT -7.   It's 07:05 AM.


Powered by vBulletin® Version 3.8.5
Copyright ©2000 - 2014, Jelsoft Enterprises Ltd.
Copyright ADVrider 2011-2014